Welding method of lamella plare clarifier
1. Open the  packaging of lamella plate clarier, the first piece inclined tube filler flat on the floor, take the second piece lamella plate placed on the first sheet, check lamella plate must ensure that 60 ° angle, and hexagonal honeycomb, check and correct contact adhesive hot start point;
2, in hexagonal honeycomb plane ends of all contacts all be hot then, both sides of the two requirements for hot flat commissure contact the above four points, two in the middle plane inclined tube filler welding requires more than four points, to ensure welding firm;
3, pay attention to rhythm when hot bonding operation, control the temperature, hot contact points to be omitted;
4, each inclined tube filler packaged as two separate contact means hot, hot followed by the completion of neatly stacked presence on the ground;
5, be sure to cut a break halfway electric iron power, and to be placed in safety.